All of our products, except “Small Bag” models comply with the following standards:

Leather

tech specs

‌Premium south American cow leather from Chile and Brazil.

Thickness: 0.8 to 1.1 mm.

Chrome-tanned.

Tear Resistance: 40 N, minimum. [Test Method: ASTM D5034 (Grab)]

Tensile Resistance: 1.4 Kgf/mm², minimum. [Test Method: ASTM D5034 (Grab)]

Color Fastness to Rubbing: Dry: Grade 4-5, gray scale, after 150 cycles. Wet: Grade 4, gray scale, after 50 cycles. [Test Method: IUF Método N°450 (US Eq: ASTM D5053)]

Total Ash (Dry Base): 6.0% maximum, including chrome. [Test Method: NCh1206 (US Eq: ASTM D2617)]

Chrome Content (Dry Base): 2.5%, minimum. [Test Method: NCh2134 (US Eq: ASTM D2807)]

Fat Content: 6.0%, minimum. [Test Method: NCh1203 (US Eq: ASTM D3495)]

Zippers & snaps

tech specs

Zippers

Brass-plated metal.
Type: Zipper, single slider, separable at the front.


Coupled Teeth: 10.0 ±1.0 mm at front and 5.0 ±1.0 mm at sleeve pocket.

ASTM D2060 for zipper testing.

Snaps

Brass-plated metal.


Diameter: 10.0 ±1.0 mm.

‌Sewing Threads

tech specs

‌Composition: 100% Polyamide or polyester, 3 strands.


Color: contrast color or similar in tone and shade to the leather.

Knit Fabric

tech specs

Composition Wool/Acrylic (50% minimum wool) ASTM D629.

Minimum Weight 180 g/m² ASTM D3776.

Average Resulting Yarn Count (Metric) 18/2 x 2 ASTM D1059.

Color: contrast color or similar in tone and shade to the leather.

Resistance to Pilling Formation, 4 hrs. Minimum ASTM D3514

Right Side 4
Reverse 4
Weave Elastic 1×1

Lining Fabric

tech specs

Composition  100% Polyamide or 100% Polyester multifilament ASTM D629.

Minimum Weight  60 g/m² ASTM D3776.

Minimum Density 42 threads/cm ASTM D3775.

Warp  34 picks/cm ASTM D5034 (Grab Method).

Weft  45 Kgf ASTM D5034 (Grab Method).

Minimum Tensile Resistance Warp 45 Kgf ASTM D5034 (Grab Method).

Weft 40 Kgf  ASTM D5034 (Grab Method).

Weave Taffeta or Twill